PETG warping and lifting out of the build plate and separating from its brim. PEI textured plate at 90C first layer 85C for the rest. is 5 degrees difference enough to cause this? Something else? #3dprinting

Replies (1)

  • @jolt@telegrafverket.cc 2026-08-03 10:47

    @NiwlCraft@mastodon.art that happens when there are long distances and the filament cools down and pulls the edges up. Try brims! Or mouse-ears if there are sharp edges (just a 1 layer circkle around where the warp happens). Using a glue-stick of some kind (made for petg of course) as a bind/release agent might help as another "throw money at the problem" option