Elektrine lite

← Feed

@tinx@jit.social

Post #1521306

2026-02-06 13:31 UTC

@cinderdazzle612 yes, it sometimes happens that the fresh filament is not properly dried. But there are other factors as well: PETG is more prone to stringing compared to PLA. It is very important not to dry the filament in an excessively hot environment. I think you should dry PLA, for example, at or below 45°C. Otherwise you might end up with a blob of fused plastic.